Discuss Galvanic Corrosion Electrical Work in the UK Electrical Forum area at ElectriciansForums.net
Zinc plating / galvanising is designed so the coating sacrifices itself to protect the base metal, such as steel, for corroding itself. Zinc is OK with aluminium, but most other metals such as stainless steel, brass and copper really go for it. Same applies if you have, say, a brass fixing on galvanised metal - it will accelerate the loss of the plating.
Fine what it is dry!Odd that we regularly use brass bushes with galv conduit fittings.
The threaded part is generally not galvanised.Odd that we regularly use brass bushes with galv conduit fittings.
But #1 rule is keep it lubricated if you ever want to change it in the future.
The threaded part is generally not galvanised.
Reply to Galvanic Corrosion Electrical Work in the UK Electrical Forum area at ElectriciansForums.net
We get it, advertisements are annoying!
Sure, ad-blocking software does a great job at blocking ads, but it also blocks useful features of our website. For the best site experience please disable your AdBlocker.